Blowing agents

The range includes endothermic and exothermic formulations as powder blends, granules or microgranulates for foaming and against collapse & warpage.
Use the following filter options for your perfect blowing agent.
(If you are looking for an additive for foaming TPE, you will find our Microspheres masterbatches here)

Reset
Art.-Nr. Name Konzentration Starttemp. Primär geeignet für Lieferform
Item no. Name Concentration Starting temp. Primarily suitable for Delivery form
1004 cell.mix 500 100,0 % 150 °C Ethylene - Copolymers, PE Powder
1211 cell.mix t062 100,0 % 145 °C PVC plastisized Powder
1215 cell.mix t100 100,0 % 150 °C Ethylene - Copolymers, PVC-U Powder
1355 cell.mix p113-c 75,0 % 150 °C PVC-U Powder
1356 cell.mix p114-c 75,0 % 165 °C PVC-U Powder
1406 cell.mix a041 30,0 % 145 °C PP, PVC plastisized Granules
1409 cell.mix a071 20,0 % 155 °C Ethylene - Copolymers, PE, PP Granules
1412 cell.mix a062 18,0 % 145 °C PA, PS Granules
1414 cell.mix pc12 12,0 % 235 °C PC Granules
1415 cell.mix a013 35,0 % 170 °C POM, PP Granules
1417 cell.mix a072 17,0 % 175 °C ABS, PE, PP, PS Granules
1421 cell.mix a085 72,0 % 150 °C ABS, Ethylene - Copolymers, PE, PP, PS Granules
1430 cell.mix a030 20,0 % 150 °C PE, PP Granules
1432 cell.mix a031 50,0 % 150 °C PE, PP Granules
1435 cell.mix a073 22,0 % 210 °C PA, POM, PP Granules
1436 cell.mix a075 70,0 % 160 °C ABS, PE, PP, PS Granules
1452 cell.mix pc12/50E 12,0 % 235 °C PC Granules
1453 cell.mix a072/50 9,0 % 170 °C PE, PP Granules
1461 cell.mix a058E 65,0 % 160 °C Ethylene - Copolymers, PE, PP Granules
1507 cell.mix a027grit 45,0 % 150 °C PVC-U Microgranules
1509 cell.mix a029grit 76,0 % 150 °C PVC-U Microgranules
1513 cell.mix a037grit 46,0 % 140 °C PVC-U Microgranules
1518 cell.mix a039grit 49,0 % 150 °C PVC-U Microgranules

Not found what you were looking for?